If code of a fracture is OFW-422 then it means.
(i) AT welding with transverse crack.
(ii) Flash butt welding with transverse crack.
(iii) At welding with horizontal crack.*
(iv) None of the above.
0 like 0 dislike

1 Answer

(iii) At welding with horizontal crack.*
0 like 0 dislike

Related questions

Where Portion sample tests(test piece) should be conducted? (i) At desire by RDSO (ii) At Zonal CMT’s organisation or the Flash Butt Welding plant. * (iii) In RDSO campus (iv) As decided by in charge of the plant
Answer : At Zonal CMT’s organisation or the Flash Butt Welding plant....

View solution
0 like 0 dislike
1 answer

Tandem rig test with 450 probe for AT weld detects. (i) Horizontal longitudinal defect in weld. (ii) Vertical oriented defect in AT weld.* (iii) Transverse defect in AT weld. (iv) Defect in flange of AT welds.
Answer : (ii) Vertical oriented defect in AT weld.*...

View solution
0 like 0 dislike
1 answer

Which gauge is used to measure the height of rail at the time of aligning of rails for AT welding? (i) Height gauge.* (ii) Vertical gauge (iii) Horizontal gauge (iv) As decided by site supervisor
Answer : (iv) As decided by site supervisor...

View solution
0 like 0 dislike
1 answer

What is the testing frequency of new AT weld ? (i) Just after the welding (ii) After 7 days of welding (iii) With in the one month of welding* (iv) None of the above
Answer : iii) With in the one month of welding*...

View solution
0 like 0 dislike
1 answer

In how many time final grinding should be done of new AT weld ? (i) Just after the welding (ii) After 8 hrs of welding (iii) With in 24 hrs* (iv) None of the above
Answer : iii) With in 24 hrs*...

View solution
0 like 0 dislike
1 answer