What is the heating time in OXY & LPG in SPW? (i) 2.0 - 3.5 minutes. (ii) 2.0 - 3.0 minutes. (iii) 2.0 - 2.5 minutes.* (iv) 3.0 - 4.5 minutes. Answer : iii) 2.0 - 2.5 minutes...
What are the recognized systems for pre heating of rails ends for AT Welding? (i) Oxygen –LPG & Compressed air petrol both* (ii) Only Oxygen –LPG (iii) Only Compressed air petrol both (iv) both are correct Answer : ) Oxygen –LPG & Compressed air petrol both*...
Pressure of Oxygen during pre-heating shall be? (i) 4.0 – 5.0 kg/ sq cm (ii) 5.0 – 6.0 kg/ sq cm (iii) 6.0 – 7.0 kg/ sq cm (iv) 7.0 – 8.0 kg/ sq cm * Answer : (iv) 7.0 – 8.0 kg/ sq cm *...
What is mould waiting time? (i) 3 to 5 minutes. (ii) 4 to 6 minutes* (iii) 3.5 to 5.5 minutes (iv) 4.5 to 6.5 minuteses Answer : (ii) 4 to 6 minutes*...
Pressure of compressed air is kept during preheating by CAPS? (i) 1 to 2 kg/cm2 (ii) .1 to .2 kg/cm2 (iii) 2 to 3 kg/cm2 (iv) 0.2 to 0.3 kg/cm2* Answer : (iv) 0.2 to 0.3 kg/cm2*...